ID:
TIME: 2018-11-26
VIEWS: 4182
Manufactured by viscose-based carbon fiber after curing stereotypes and the second high-temperature processing by purification. It has good performance of anti-ablation, thermal shock resistance, erosion resistance and long lifespan.
Lighter and higher temperature resistant than PAN-based. Better used in Semiconductor industry or High-end materials for Electronics.
Grade | JP-SFR-14(Rayon-based) | JP-SFR-24(Rayon-based) | |
Bulk Density (g/cm^3) | 0.08—0.14 | 0.06—0.10 | |
Carbon content(%) | ≥98 | ≥99 | |
Ash (%) | 0.05% | 0.005% | |
Thermal Conductivity (W/m·k) 1150℃ | 0.10—0.16 | 0.06—0.14 | |
Tensile strength (MPa) | 0.13 | 0.1 | |
Crushing stress at10% compression(N/cm2) | 6—10 | 5—8 | |
Process Temperature(℃) | 1400 | 2400 | |
Operation Temperature | Atmosphere(℃) | ≤400 | ≤400 |
Vacuum(℃) | ≤1600 | ≤2200 | |
Inert Gas(℃) | ≤2200 | ≤3400 | |
Length(Meter) | 13—20 | 13—20 | |
Width(mm) | 1000—1200 | 1000—1200 | |
Thickness(mm) | 3, 5 ,8, 10 | 3, 5 ,8, 10 |